Search for collections on University of Merdeka Malang Repository

Penggunaan Limbah Kaca Bening Bangunan Sebagai (Fiiler) dalam Campuran AC-WC (Asphalt Concrete-Wearning Course) pada Jalan Raya Perkerasan Aspal Panas

Martins, Agustinho L. V. (2022) Penggunaan Limbah Kaca Bening Bangunan Sebagai (Fiiler) dalam Campuran AC-WC (Asphalt Concrete-Wearning Course) pada Jalan Raya Perkerasan Aspal Panas. Undergraduate thesis, Fakultas Teknik Universitas Merdeka Malang.

[thumbnail of COVER.pdf]
Preview
Text
COVER.pdf

Download (1MB) | Preview
[thumbnail of BAB I.pdf]
Preview
Text
BAB I.pdf

Download (117kB) | Preview
[thumbnail of BAB II.pdf] Text
BAB II.pdf
Restricted to Repository staff only

Download (293kB)
[thumbnail of BAB III.pdf] Text
BAB III.pdf
Restricted to Repository staff only

Download (356kB)
[thumbnail of BAB IV.pdf] Text
BAB IV.pdf
Restricted to Repository staff only

Download (815kB)
[thumbnail of BAB V.pdf] Text
BAB V.pdf
Restricted to Repository staff only

Download (47kB)
[thumbnail of DAFTAR PUSTAKA.pdf]
Preview
Text
DAFTAR PUSTAKA.pdf

Download (85kB) | Preview
[thumbnail of HASIL CEK PLAGIASI.pdf]
Preview
Text
HASIL CEK PLAGIASI.pdf

Download (1MB) | Preview

Abstract

AC-WC is a layer on road pavement construction consisting of: from a mixture of hard asphalt which has a continuous gradation, mixed, mixed spread and solidified at a certain temperature.according to the specifications of Bina Marga 2010 revision 3, all asphalt mixtures must contain fillers.
The filler used in this study is glass waste from Clear Glass Refining This study aims to determine the percentage of glass waste filler that optimum and its effect on the performance of the mixture. From Correlation results in terms of the 100% rock ash filler shown on the composite graph, at variation of 100% Clear glass filler stability value decreased -2.06%, at 25% filler variation Clear glass stability value has increased 12.61%, at 50% filler variation. Clear glass stability value experienced an increase of 1.73%, at 75% filler variation Clear glass stability value experienced an increase of 5.20%. As for the value of the melt (flow), at 100% clear glass filler, the melting value (flow) has increased by 6.80%, at 25% filler variation Clear glass the melting value (flow) has decreased -5.32%, at 50% filler variation. Clear glass, the melting value (flow) experienced an increase of 35.50%, filler variation 75% Clear glass melting value (flow) decreased -5.63%.
Based on the results of the Marshall test, the mixture with this proportion is more resistant to water immersion so it has higher durability and is more durable resistant to potential disintegration.

Item Type: Thesis (Undergraduate)
Additional Information: Agustinho L. V. Martins NIM : 14410008
Uncontrolled Keywords: AC-WC, Fine Aggregate, Clear Glass, Marshall
Subjects: T Technology > TA Engineering (General). Civil engineering (General)
T Technology > TE Highway engineering. Roads and pavements
Divisions: Fakultas Teknik > S1 Teknik Sipil
Depositing User: Gendhis Dwi Aprilia
Date Deposited: 15 Feb 2025 07:26
Last Modified: 15 Feb 2025 08:31
URI: https://eprints.unmer.ac.id/id/eprint/4292

Actions (login required)

View Item View Item